Manufacturer, stockist and exporter, supplying worldwide from Mumbai, India yash@aerosteel.co.in+91 78748 73449WhatsApp

Duplex 2205 vs super duplex 2507 vs 316L

Strength, pitting resistance and temperature limits compared, so you can decide when to move beyond 316L.

By the technical team at Aero Steel Overseas. Updated 2026-11-01.

When 316L starts to pit or crack in chloride service, engineers usually look at duplex stainless steel next. This guide compares 316L, duplex 2205 and super duplex 2507 on corrosion resistance, strength and practical limits.

Side-by-side comparison

Property316LDuplex 2205Super duplex 2507
UNSS31603S31803 / S32205S32750
MicrostructureAusteniticAustenite + ferriteAustenite + ferrite
Approx. PREN243542 or above
Min. yield strength, pipe (MPa)170450–485550
Chloride stress corrosion crackingSusceptible above about 50 °CMuch betterExcellent
Practical temperature rangeCryogenic to high temperatureAbout −50 °C to 250–300 °CAbout −50 °C to 250 °C
Typical usesChemical, pharma, food, marine atmosphereOil and gas, desalination, pulp and paperSeawater, offshore, firewater, sour service

Strength values are minimums for pipe under ASTM A312 and A790. Check the standard on your order.

Why duplex is stronger

The two-phase structure roughly doubles yield strength compared with austenitic grades. In pressure piping this allows a thinner wall for the same design pressure, which saves weight and often offsets the higher price per kilogram.

Corrosion resistance

Higher chromium, molybdenum and nitrogen give duplex grades a higher PREN, so they resist pitting and crevice corrosion in conditions that attack 316L. The ferrite phase also makes them far more resistant to chloride stress corrosion cracking. Super duplex is generally the minimum for warm seawater.

Limits to keep in mind

  • Temperature: long exposure above about 300 °C causes 475 °C embrittlement, so duplex is not used for hot service.
  • Welding: qualified procedures must control heat input to keep the ferrite-austenite balance and avoid intermetallic phases.
  • Availability: fittings and flanges in super duplex can have longer lead times than 316L; plan them early.

Matching components

Duplex 2205 pipe (ASTM A790) is matched with A815 WPS32205 fittings and A182 F51 or F60 flanges. Super duplex S32750 uses A815 WPS32750 fittings and F53 flanges; S32760 uses F55.

See our duplex and super duplex range, or compare with 304 and 316 stainless.